APTIV® 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 2000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.


Please note - APTIV 2000 will crystallise if taken above the Tg [143°C (289°F)] in either secondary processes or end use application. The crystallisation is not reversible back to the amorphous phase without re-melting the material. Consideration of the temperature range during processing and end use application needs to be included if selecting APTIV 2000.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.26 g/cm³

Show Material materials with Dichte of 1.26 g/cm³

ISO 1183

Wasserabsorption

23.0 °C

0.21 %

Show Material materials with Wasserabsorption of 0.21 %

ISO 62 (50% RH, 24h)

Abmessung

PropertyValue

Dicke

0.05 mm

Show Material materials with Dicke of 0.05 mm

Mechanisch

PropertyTemperatureValueComment

Dehnung

23.0 °C

200 %

Show Material materials with Dehnung of 200 %

ISO 527

Dehnung, transversal

23.0 °C

200 %

Show Material materials with Dehnung, transversal of 200 %

ISO 527

Durchschlagfestigkeit

23.0 °C

470 kJ/m²

Show Material materials with Durchschlagfestigkeit of 470 kJ/m²

Def Stan 81-75

Elastizitätsmodul

23.0 °C

1.8 GPa

Show Material materials with Elastizitätsmodul of 1.8 GPa

ISO 527

Elastizitätsmodul, transversal

23.0 °C

1.8 GPa

Show Material materials with Elastizitätsmodul, transversal of 1.8 GPa

ISO 527

Reißfestigkeit

23.0 °C

6 kN/m

Show Material materials with Reißfestigkeit of 6 kN/m

ISO 6383-1

Reißfestigkeit, transversal

23.0 °C

6 kN/m

Show Material materials with Reißfestigkeit, transversal of 6 kN/m

ISO 6383-1

Zugfestigkeit

23.0 °C

120 MPa

Show Material materials with Zugfestigkeit of 120 MPa

ISO 527

Zugfestigkeit, transversal

23.0 °C

120 MPa

Show Material materials with Zugfestigkeit, transversal of 120 MPa

ISO 527

Thermisch

PropertyTemperatureValueComment

Glasübergangstemperatur

143 °C

Show Material materials with Glasübergangstemperatur of 143 °C

Koeffizient der thermischen Ausdehnung

23.0 °C

6E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 6E-5 1/K

ASTM D696 (below Tg)

Elektrisch

PropertyTemperatureValueComment

Dielektrizitätskonstante

23.0 °C

3 [-]

Show Material materials with Dielektrizitätskonstante of 3 [-]

ASTM D150 (10MHz)

Durchschlagfestigkeit

23.0 °C

190 kV/mm

Show Material materials with Durchschlagfestigkeit of 190 kV/mm

ASTM D149 (6.25mm electrode)

Durchschlagspannung

23.0 °C

9.5 kV

Show Material materials with Durchschlagspannung of 9.5 kV

ASTM D149 (6.25mm electrode)

Verlustfaktor

23.0 °C

3E-3 [-]

Show Material materials with Verlustfaktor of 3E-3 [-]

ASTM D150 (10Mhz)

spezifischer Widerstand

23.0 °C

2.00E+14 Ω·m

Show Material materials with spezifischer Widerstand of 2.00E+14 Ω·m

ASTM D257 (100V)

Rheological Properties

PropertyTemperatureValueComment

Schrumpfung

200.0 °C

10 %

Show Material materials with Schrumpfung of 10 %

TM-VX-84

Schrumpfung, diagonal

200.0 °C

5 %

Show Material materials with Schrumpfung, diagonal of 5 %

TM-VX-84

Technological properties

Property
Application areas

Aerospace insulation, electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts, composites

Certifications

APTIV 2000 film is approved for Food Contact Use: APTIV 2000 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2000 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2000 film is fully compliant with the 3-A Sanitary Standards. APTIV film 2000 complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2000 film is inherently halogen-free in accordance with IEC61249-2-21.

Other

The key features are: High heat resistance, excellent Flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process.

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. APTIV 2000 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms: Surface treatment, adhesion, coatings, slitting, die cutting and stamping, thermal lamination, heat welding and heat sealing, metallisation, laser marking and machining, thermoforming, printing