Abmessung
Property | Value |
---|---|
Dicke | 0.13 mm Show Material materials with Dicke of 0.13 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 150 % Show Material materials with Dehnung of 150 % | ISO 527 |
Dehnung, transversal | 23.0 °C | 150 % Show Material materials with Dehnung, transversal of 150 % | ISO 527 |
Elastizitätsmodul | 23.0 °C | 3 GPa Show Material materials with Elastizitätsmodul of 3 GPa | ISO 527 |
Elastizitätsmodul, transversal | 23.0 °C | 3 GPa Show Material materials with Elastizitätsmodul, transversal of 3 GPa | ISO 527 |
Zugfestigkeit | 23.0 °C | 100 MPa Show Material materials with Zugfestigkeit of 100 MPa | ISO 527 |
Zugfestigkeit, transversal | 23.0 °C | 80 MPa Show Material materials with Zugfestigkeit, transversal of 80 MPa | ISO 527 |
Thermisch
Property | Value |
---|---|
Glasübergangstemperatur | 143 °C Show Material materials with Glasübergangstemperatur of 143 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts | |
Certifications | APTIV 2100 film is approved for food contact Use: APTIV 2100 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2100 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2100 film complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2100 film is inherently halogen-free in accordance with IEC61249-2-21. | |
Other | The key features are: High heat resistance, excellent flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable, excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties and barrier properties, high purity, lightweight, recyclable, easy to process. | |
Processing methods | Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. |