Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.94 g/cm³ Show Supplier Material materials with Dichte of 0.94 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.23 - 0.88 GPa Show Supplier Material materials with Biegemodul of 0.23 - 0.88 GPa | ASTM D790 |
Dehnung | 23.0 °C | 110 - 350 % Show Supplier Material materials with Dehnung of 110 - 350 % | ASTM D638 |
Härte, Shore D | 23.0 °C | 58 [-] Show Supplier Material materials with Härte, Shore D of 58 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 220 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 220 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 20.5 - 21 MPa Show Supplier Material materials with Streckgrenze of 20.5 - 21 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 11.75 MPa Show Supplier Material materials with Zugfestigkeit of 11.75 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 118 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 118 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 3.8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 3.8 g/10min | ASTM D1238, 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its combination of mechanical properties, ESCR resistance and fluidity, GREENETHENE G-3938 is suggested for the production of wide variety of tank applications for the storage of water, chemicals & Oils. GREENETHENE G-3938 can also be used for off-shore flotation buoys and road crash barriers. | |
Certifications | List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996 | |
Color | Natural, black, terracotta, fire red, yellow and blue. | |
Processing methods | Compression molded & rotomolded |