Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.94 g/cm³ Show Supplier Material materials with Dichte of 0.94 g/cm³ | ASTM D1505 |
Schüttdichte | 23.0 °C | 450 g/cm³ Show Supplier Material materials with Schüttdichte of 450 g/cm³ | ASTM D1525 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.25 - 0.75 GPa Show Supplier Material materials with Biegemodul of 0.25 - 0.75 GPa | ASTM D790 |
Dehnung | 23.0 °C | 250 - 950 % Show Supplier Material materials with Dehnung of 250 - 950 % | ASTM D638 |
Härte, Shore D | 23.0 °C | 57 [-] Show Supplier Material materials with Härte, Shore D of 57 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 500 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 500 J/m | ASTM D256, Partial Break |
Streckgrenze | 23.0 °C | 19.75 - 20 MPa Show Supplier Material materials with Streckgrenze of 19.75 - 20 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 12.25 MPa Show Supplier Material materials with Zugfestigkeit of 12.25 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 118 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 118 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 4 g/10min | ASTM D1238, 190°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its combination of mechanical properties, ESCR resistance & fluidity, GREENETHENE G-3904U is suggested for the production of Playground equipment, manholes, storage containers, chemical & Oil tanks. | |
Certifications | List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996 | |
Processing methods | Compression molded & rotomolded |