Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.94 g/cm³ Show Supplier Material materials with Dichte of 0.94 g/cm³ | ASTM D794 |
Moisture absorption | 23.0 °C | 0.02 % Show Supplier Material materials with Moisture absorption of 0.02 % | ASTM D6982, 100°C - 1hr |
Mechanisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.4 g/10min | ASTM D1238, 190°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | Irrigation Hoses - Film Grade | |
Color | Orange |