Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.99 g/cm³ Show Supplier Material materials with Dichte of 0.99 g/cm³ | ASTM D798 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ASTM D6982, 100°C - 1hr |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 10 % Show Supplier Material materials with Aschegehalt of 10 % | max., ASTM D5630 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.3 - 0.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.3 - 0.9 g/10min | ASTM D1238, 190°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | Film, sheet, shopping bag, irrigation tube and electrical hose. | |
Color | Grey |