Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 0.17 GPa Show Supplier Material materials with Biegemodul of 0.17 GPa | ISO178 | ||
Härte, Shore D | 23.0 °C | 52 - 53 [-] Show Supplier Material materials with Härte, Shore D of 52 - 53 [-] | ISO868 | ||
Zugfestigkeit | 23.0 °C | 52 MPa Show Supplier Material materials with Zugfestigkeit of 52 MPa | ISO527 | ||
Schlagfestigkeit, Charpy gekerbt | ISO179, No break @-30, 23°C |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 158 °C Show Supplier Material materials with Schmelzpunkt of 158 °C | ISO11357 |
Technological properties
Property | ||
---|---|---|
Application areas | Glass frames, eyeglasses frames, eyeglasses, sports sunglasses, watches, headphones, water cups, precipitation cups, filter cups, water-oil separators, fuel filter, filter filters, baby bottles, tea cups, edible oil bottles, cosmetics containers, dashboards, milk machinery shells, eyeglasses, water filter bowls, filter coverage, pneumatic air bowls. |