Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 13 MPa Show Supplier Material materials with Biegefestigkeit of 13 MPa | ISO178 | ||
Biegemodul | 23.0 °C | 0.28 GPa Show Supplier Material materials with Biegemodul of 0.28 GPa | ISO178 | ||
Dehnung | 23.0 °C | 300 % Show Supplier Material materials with Dehnung of 300 % | ISO527 | ||
Härte, Shore D | 23.0 °C | 58 - 60 [-] Show Supplier Material materials with Härte, Shore D of 58 - 60 [-] | ISO868 | ||
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 35 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 35 kJ/m² | ISO179 | ||
23.0 °C | 60 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 60 kJ/m² | ISO179 | |||
Streckgrenze | 23.0 °C | 18 MPa Show Supplier Material materials with Streckgrenze of 18 MPa | ISO527 | ||
Zugfestigkeit | 23.0 °C | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | ISO527 | ||
Schlagzähigkeit, Charpy ungekerbt | ISO179, No break @-30, 23°C |
Technological properties
Property | ||
---|---|---|
Application areas | Nylon badmintion, shuttlecock | |
Processing methods | Drying Temperature: 75-80°C, Drying Time: 3-4 hr, Rear Temperature: 180°C, Middle Temperature: 250°C, Front Temperature: 250°C, Nozzle Temperature: 230°C, Mold Temperature: 60-80°C, Injection Pressure: 70-100 MPa |