Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Biegefestigkeit of 65 MPa | ISO178 | ||
Biegemodul | 23.0 °C | 1.6 GPa Show Supplier Material materials with Biegemodul of 1.6 GPa | ISO178 | ||
Dehnung | 23.0 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO527 | ||
Elastizitätsmodul | 23.0 °C | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | ISO527 | ||
Hardness, Ball Indentation | 23.0 °C | 90 MPa Show Supplier Material materials with Hardness, Ball Indentation of 90 MPa | ISO2039-1 | ||
Härte, Shore D | 23.0 °C | 82 [-] Show Supplier Material materials with Härte, Shore D of 82 [-] | ISO868 | ||
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | ISO179 | ||
23.0 °C | 14 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14 kJ/m² | ISO179 | |||
Zugfestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | ISO527 | ||
Schlagzähigkeit, Charpy ungekerbt | No break @-30, 23°C |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Memory glasses frame, headphones, cosmetic; Electronic connector, infrared sensor cover, mobile, phone shell; Oil cup, clasp, handle, flowmeter, observing Mirror/Window, Oil nozzle cover, milker; Sanitary ware: bracket, water pipe/pressure regulating valve, water filter, window, flowmeter; Food containers: drinking cups, transparent containers, transparent tableware; Motion device: diving device shield, knife handle, waterproof watch case; Medical devices: Protective mask mirror, hearing aid/earphone/ear hang, respiratory mask | |
Processing methods | Drying Temperature: 90-100°C, Drying Time: 6-8 hr, Rear Temperature: 200°C, Middle Temperature: 240°C, Front Temperature: 250°C, Nozzle Temperature: 240°C, Mold Temperature: 60-90°C, Injection Pressure: 80-100 MPa |