Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Supplier Material materials with Dichte of 1.02 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dehnung | 23.0 °C | 100 % Show Supplier Material materials with Dehnung of 100 % | ISO527 | ||
Elastizitätsmodul | 23.0 °C | 0.5 GPa Show Supplier Material materials with Elastizitätsmodul of 0.5 GPa | ISO527 | ||
Härte, Shore D | 23.0 °C | 62 [-] Show Supplier Material materials with Härte, Shore D of 62 [-] | ISO868 | ||
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | ISO179, No break @-30°C | ||
Streckgrenze | 23.0 °C | 26 MPa Show Supplier Material materials with Streckgrenze of 26 MPa | ISO527 | ||
Zugfestigkeit | 23.0 °C | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | ISO527 | ||
Schlagzähigkeit, Charpy ungekerbt | No break @-30, 23°C |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 32 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 32 kV/mm | IEC60243-1 |
Kriechstromfestigkeit | 23.0 °C | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC60112 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC60093 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.9 - 1.3 % Show Supplier Material materials with Schrumpfung of 0.9 - 1.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Oil tube, corrugated tube | |
Processing methods | Drying Temperature: 80-85°C, Drying Time: 4-6 hr, Rear Temperature: 200°C, Middle Temperature: 210°C, Front Temperature: 220°C, Nozzle Temperature: 230°C |