Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 25 % Show Supplier Material materials with Dehnung A5 of 25 % | min. |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Supplier Material materials with Elastizitätsmodul of 200 GPa | |
Härte, Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, Brinell of 270 [-] | max. |
Streckgrenze Rp 0,2 | 23.0 °C | 500 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 500 MPa | min. |
Zugfestigkeit | 23.0 °C | 700 - 900 MPa Show Supplier Material materials with Zugfestigkeit of 700 - 900 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 15 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 15 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 8E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 8E-7 Ω·m |
Magnetisch
Property | Value |
---|---|
Magnetic properties | Magnetisation very low |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Kupfer | 1 - 2.5 % Show Supplier Material materials with Kupfer of 1 - 2.5 % | |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Molybdän | 3 - 4 % Show Supplier Material materials with Molybdän of 3 - 4 % | |
Nickel | 6 - 8 % Show Supplier Material materials with Nickel of 6 - 8 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Stickstoff | 0.2 - 0.3 % Show Supplier Material materials with Stickstoff of 0.2 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical & petrochemical, Ship building industry, Apparatus and tank construction, Turbine construction, Power plant construction, Transformer construction, Power engineering for onshore and offshore, Plant construction, Mechanical Engineering, Food industry | |
Corrosion properties | Very good corrosion and chemical resistance | |
General machinability | Good | |
Polishing ability | Good | |
Solution annealing | 1040-1120°C | |
Wear resistance | High resistance | |
Welding | TIG welding: limited, MAG Solid wire: limited, Arc welding: limited, UP welding: unsuitable, Laser beam welding: limited, Gas fusion welding: unsuitable | |
Workability | Hot forming: 1000-1200°C |