Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 10 % Show Supplier Material materials with Dehnung A5 of 10 % | min. |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Supplier Material materials with Elastizitätsmodul of 200 GPa | |
Härte, Brinell | 23.0 °C | 440 [-] Show Supplier Material materials with Härte, Brinell of 440 [-] | max. |
Streckgrenze Rp 0,2 | 23.0 °C | 720 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 720 MPa | min. |
Zugfestigkeit | 23.0 °C | 930 - 1200 MPa Show Supplier Material materials with Zugfestigkeit of 930 - 1200 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 11 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 11 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 7.7E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 7.7E-7 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15 - 15.5 % Show Supplier Material materials with Chrom of 15 - 15.5 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 2.5 - 4.5 % Show Supplier Material materials with Kupfer of 2.5 - 4.5 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Nickel | 3.5 - 4.5 % Show Supplier Material materials with Nickel of 3.5 - 4.5 % | |
Niobium | 0.15 - 0.49 % Show Supplier Material materials with Niobium of 0.15 - 0.49 % | Nb+Ta |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Mechanical Engineering, Power Engineering, Plant construction, Chemistry Offshore | |
Corrosion properties | Good | |
Welding | Good |