Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.9 g/cm³ Show Supplier Material materials with Dichte of 0.9 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.88 GPa Show Supplier Material materials with Biegemodul of 0.88 GPa | ASTM D790 |
Hardness, Rockwell R | 23.0 °C | 75 [-] Show Supplier Material materials with Hardness, Rockwell R of 75 [-] | ASTM D785 |
Impact strength, Izod unnotched, ASTM | -10.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 26.48 MPa Show Supplier Material materials with Streckgrenze of 26.48 MPa | ASTM D638 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 90 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 90 °C | ASTM D648 | |
Koeffizient der thermischen Ausdehnung | 80.0 °C | 1.5E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-4 1/K | Mean value between 0°C and the mentioned temperature, Dilatometer |
Schmelzpunkt | 141 °C Show Supplier Material materials with Schmelzpunkt of 141 °C | ASTM D3418 | |
Vicat-Erweichungstemperatur | 130 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 130 °C | ASTM D1525 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | Minimum, ASTM HS Method |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.25 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.25 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Pipes and fittings, piping for house, radiator pipes, idustrial pipes |