Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.9 g/cm³ Show Supplier Material materials with Dichte of 0.9 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.47 GPa Show Supplier Material materials with Biegemodul of 1.47 GPa | ASTM D790 |
Hardness, Rockwell R | 23.0 °C | 85 [-] Show Supplier Material materials with Hardness, Rockwell R of 85 [-] | ASTM D785 |
Impact strength, Izod unnotched, ASTM | -10.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 50 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 31.38 MPa Show Supplier Material materials with Streckgrenze of 31.38 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 166 °C Show Supplier Material materials with Schmelzpunkt of 166 °C | ASTM D3418 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.3 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.3 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Sewer/drainage pipes (solid wall type-corrugated type), storm water drainage system |