В180 is a prepreg based on epoxy resin and reinforcing filler (unidirectional tapes or fabrics of various weaving) for producing details with operating temperatures up to 150°C. Out-of-autoclave prepreg technology has the most advantages of autoclave. The autoclave is not required for processing the prepreg B180. Curing takes place in a vacuum bag, with the technology of the package laminating slightly different from the vacuum infusion. It shows the following features and properties:


  • High mechanical performance
  • Possibility of application in loaded parts at service temperatures up to 120°C
  • Less stringent requirements for working staff
  • Glass transition temperature 154°C
  • Out of autoclave processing
  • Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Allgemein

    PropertyTemperatureValueComment

    Wasserabsorption

    23.0 °C

    4.17 %

    Show Material materials with Wasserabsorption of 4.17 %

    for 54h to boiling water

    Mechanisch

    PropertyTemperatureValueComment

    Biegefestigkeit

    23.0 °C

    162 MPa

    Show Material materials with Biegefestigkeit of 162 MPa

    ASTM D790

    Plane-Strain Fracture Toughnes

    23.0 °C

    1.88 MPa·√m

    Show Material materials with Plane-Strain Fracture Toughnes of 1.88 MPa·√m

    ASTM D5045

    Zugfestigkeit

    23.0 °C

    94 MPa

    Show Material materials with Zugfestigkeit of 94 MPa

    ASTM D638

    Formänderungsenergieabgabe

    ASTM D5045

    Thermisch

    PropertyValueComment

    Glasübergangstemperatur

    175 °C

    Show Material materials with Glasübergangstemperatur of 175 °C

    ASTM E2092

    Technological properties

    Property
    Application areas

    Marine: The shells of boats and sport catamarans can be made of composites;Car tuning: The composite material provides solutions for automotive parts to be light-weighted, stylish and aesthetic;Sports equipment: Frame, wheels, seat, seat post, handlebar, head stem and crank arm of a sports bicycle are made of carbon composite

    Processing methods

    Holding at a temperature of 25-30°C, for 12 hours, a vacuum of -1 bar. Heating 2°C/min. up to 120°C, holding at 120°C for 180 minutes. Heating 2°C/min. up to 180°C, holding at 180°C for 180 minutes, cooling no faster than 5°C/min. up to 50°С.