Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 - 15 % Show Supplier Material materials with Dehnung of 10 - 15 % |
Elastizitätsmodul | 23.0 °C | 100 GPa Show Supplier Material materials with Elastizitätsmodul of 100 GPa |
Härte, Brinell | 23.0 °C | 149 - 212 [-] Show Supplier Material materials with Härte, Brinell of 149 - 212 [-] |
Härte, Rockwell C | 23.0 °C | 0 - 18 [-] Show Supplier Material materials with Härte, Rockwell C of 0 - 18 [-] |
Härte, Vickers | 23.0 °C | 150 - 220 [-] Show Supplier Material materials with Härte, Vickers of 150 - 220 [-] |
Streckgrenze | 23.0 °C | 300 - 670 MPa Show Supplier Material materials with Streckgrenze of 300 - 670 MPa |
Zugfestigkeit | 23.0 °C | 600 - 750 MPa Show Supplier Material materials with Zugfestigkeit of 600 - 750 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Blei | 0.09 % Show Supplier Material materials with Blei of 0.09 % | max. |