Quick Comparison

Other Copper Zinc Alloy

EN 1652 Grade CuZn20Al2As R390

Other Copper Zinc Alloy

EN 12452 Grade CuZn20Al2As O60

Other Copper Zinc Alloy

EN 1652 Grade CuZn20Al2As R330

Other Copper Zinc Alloy

EN 12163 Grade CuZn31Si1 R460

Other Copper Zinc Alloy

EN 12163 Grade CuZn31Si1 R530

Other Copper Zinc Alloy

EN 12163 Grade CuZn40Mn2Fe1 R460

Other Copper Zinc Alloy

EN 12163 Grade CuZn40Mn2Fe1 R540

Other Copper Zinc Alloy

EN 12163 Grade CuZn31Si1 H115

Other Copper Zinc Alloy

EN 12163 Grade CuZn31Si1 H140