Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 119 MPa Show Supplier Material materials with Biegefestigkeit of 119 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.46 GPa Show Supplier Material materials with Biegemodul of 3.46 GPa | ASTM D790 |
Dehnung | 23.0 °C | 3.3 % Show Supplier Material materials with Dehnung of 3.3 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 4.1 GPa Show Supplier Material materials with Elastizitätsmodul of 4.1 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 204 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 204 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 97 MPa Show Supplier Material materials with Zugfestigkeit of 97 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 145 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 145 °C | ASTM D648 | |
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 - 0.5 % Show Supplier Material materials with Schrumpfung of 0.3 - 0.5 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal, Washing machine drum, Water pump parts, Water treatment components, Furniture parts. | |
Color | Natural, and custom colors | |
Fillers | 20% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C, Moisture Content 0.02%, Dew Point -29°C |