Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 139 MPa Show Supplier Material materials with Biegefestigkeit of 139 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.97 GPa Show Supplier Material materials with Biegemodul of 3.97 GPa | ASTM D790 |
Dehnung | 23.0 °C | 6.7 % Show Supplier Material materials with Dehnung of 6.7 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 4.3 GPa Show Supplier Material materials with Elastizitätsmodul of 4.3 GPa | ASTM D638 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 29 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 29 kJ/m² | ISO 179 |
Zugfestigkeit | 23.0 °C | 109 MPa Show Supplier Material materials with Zugfestigkeit of 109 MPa | ASTM D638 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 - 0.5 % Show Supplier Material materials with Schrumpfung of 0.3 - 0.5 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal, Washing machine drum, Water pump parts, Water treatment components, Furniture parts. | |
Fillers | 20% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C, Moisture Content 0.02%, Dew Point -29°C |