Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.48 g/cm³ Show Supplier Material materials with Dichte of 1.48 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 191 MPa Show Supplier Material materials with Biegefestigkeit of 191 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 11.87 GPa Show Supplier Material materials with Biegemodul of 11.87 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1.1 % Show Supplier Material materials with Dehnung of 1.1 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 13.56 GPa Show Supplier Material materials with Elastizitätsmodul of 13.56 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 217 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 217 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 157 MPa Show Supplier Material materials with Zugfestigkeit of 157 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 154 °C | ASTM D648 | |
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal and Washing machine drum | |
Color | Natural, and custom colors | |
Fillers | 60% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 210 - 249 °C, Mould temperature 38 - 77 °C, Pre-drying 4 hrs @ 82 °C |