Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 275 MPa Show Supplier Material materials with Biegefestigkeit of 275 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 19.85 GPa Show Supplier Material materials with Biegemodul of 19.85 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1 - 2 % Show Supplier Material materials with Dehnung of 1 - 2 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 20.15 GPa Show Supplier Material materials with Elastizitätsmodul of 20.15 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 152 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 152 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 530 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 530 J/m | ASTM D4812 |
Zugfestigkeit | 23.0 °C | 205 MPa Show Supplier Material materials with Zugfestigkeit of 205 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 100 - 10000 Ω/sq Show Supplier Material materials with Surface resistivity of 100 - 10000 Ω/sq | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Color | Natural, and custom colors | |
Fillers | 30% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 80 - 125 MPa, Melt Temperature 320 - 350 °C, Mould temperature 120 - 175 °C, Pre-drying 3 hrs @ 120 °C, Moisture Content 0.05% |