Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 327 MPa Show Supplier Material materials with Biegefestigkeit of 327 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 14.03 GPa Show Supplier Material materials with Biegemodul of 14.03 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 16.76 GPa Show Supplier Material materials with Elastizitätsmodul of 16.76 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 327 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 327 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 253 MPa Show Supplier Material materials with Zugfestigkeit of 253 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 249 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 249 °C | ASTM D648 | |
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.2 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Suitable for automotive (Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end), electronic appliances, sport equipment, power tools, tool handles, high speed rail accessories and etc. | |
Color | Natural, and custom colors | |
Fillers | 50% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 34 - 124 MPa, Melt Temperature 271 - 299 °C, Mould temperature 66 - 124 °C, Pre-drying 2-4 hrs @ 79 °C, Moisture Content 0.20%, Dew Point -18°C |