Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.68 g/cm³ Show Supplier Material materials with Dichte of 1.68 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 333 MPa Show Supplier Material materials with Biegefestigkeit of 333 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 18.86 GPa Show Supplier Material materials with Biegemodul of 18.86 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 23.13 GPa Show Supplier Material materials with Elastizitätsmodul of 23.13 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 316 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 316 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 237 MPa Show Supplier Material materials with Zugfestigkeit of 237 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.2 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.2 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, Power tool housing, High-speed rail accessories, Water pump impeller, Washing machine drum, gears, Automotive: Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end | |
Color | Natural, and custom colors | |
Fillers | 60% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 243 - 271 °C, Mould temperature 54 - 93 °C, Pre-drying 2 hrs @ 82 °C, Moisture Content 0.20%, Dew Point -29°C |