Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Dichte of 1.56 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 316 MPa Show Supplier Material materials with Biegefestigkeit of 316 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 12.19 GPa Show Supplier Material materials with Biegemodul of 12.19 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2.2 % Show Supplier Material materials with Dehnung of 2.2 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 16.93 GPa Show Supplier Material materials with Elastizitätsmodul of 16.93 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 304 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 304 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 220 MPa Show Supplier Material materials with Zugfestigkeit of 220 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, Power tool housing, High-speed rail accessories, Water pump impeller, Washing machine drum, gears, Automotive: Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end | |
Color | Natural, and custom colors | |
Fillers | 50% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 243 - 271 °C, Mould temperature 54 - 93 °C, Pre-drying 2 hrs @ 82 °C, Moisture Content 0.20%, Dew Point -29°C |