Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 111.7 MPa Show Supplier Material materials with Biegefestigkeit of 111.7 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 7.11 GPa Show Supplier Material materials with Biegemodul of 7.11 GPa | ASTM D790 |
Dehnung | 23.0 °C | 3.4 % Show Supplier Material materials with Dehnung of 3.4 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 38.49 GPa Show Supplier Material materials with Elastizitätsmodul of 38.49 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 109 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 109 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 84 MPa Show Supplier Material materials with Zugfestigkeit of 84 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Used for automotive interior decoration, power tools, sports equipment, lawnmowers and snow blowers, industrial parts, office equipment housings, etc . | |
Color | Natural, and custom colors | |
Fillers | 30% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 70 - 110 MPa, Melt Temperature 210 - 240 °C, Mould temperature 60 - 90 °C, Pre-drying 2- 4 hrs @ 80 - 95 °C, Moisture Content 0.01% |