Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 179 MPa Show Supplier Material materials with Biegefestigkeit of 179 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 8.27 GPa Show Supplier Material materials with Biegemodul of 8.27 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1.5 - 2.5 % Show Supplier Material materials with Dehnung of 1.5 - 2.5 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 8.96 GPa Show Supplier Material materials with Elastizitätsmodul of 8.96 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 267 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 267 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 908 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 908 J/m | ASTM D4812 |
Zugfestigkeit | 23.0 °C | 121 MPa Show Supplier Material materials with Zugfestigkeit of 121 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 154 °C | ASTM D648 | |
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | For Automotive Industry: Bumper support, Spare tire holder, Door Sills, Noise encapsulation, Front ends, Seat structures, Under body panels and Dashboard, Cooling fan and frame, Battery bracket, Engine cover, Foot pedal, Washing machine drum, Water pump parts, Water treatment components, Furniture parts. | |
Color | White/Also as required | |
Fillers | 45% Long Glass Fiber | |
Processing methods | Injection Molding |