Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Dichte of 1.37 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 276 MPa Show Supplier Material materials with Biegefestigkeit of 276 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 9.65 GPa Show Supplier Material materials with Biegemodul of 9.65 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2 - 3 % Show Supplier Material materials with Dehnung of 2 - 3 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 10.34 GPa Show Supplier Material materials with Elastizitätsmodul of 10.34 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 187 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 187 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 801 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 801 J/m | ASTM D4812 |
Zugfestigkeit | 23.0 °C | 179 MPa Show Supplier Material materials with Zugfestigkeit of 179 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 249 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 249 °C | ASTM D648 | |
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.2 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Suitable for automotive (Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end), electronic appliances, sport equipment, power tools, tool handles, high speed rail accessories and etc. | |
Color | Natural/Also as required | |
Fillers | 33% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 277 - 299 °C, Mould temperature 66 - 107 °C, Pre-drying 4 hrs @ 79 °C, Moisture Content 0.2%, Dew Point -18°C |