Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Dichte of 1.46 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 255 MPa Show Supplier Material materials with Biegefestigkeit of 255 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 8.28 GPa Show Supplier Material materials with Biegemodul of 8.28 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2 - 3 % Show Supplier Material materials with Dehnung of 2 - 3 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 11.72 GPa Show Supplier Material materials with Elastizitätsmodul of 11.72 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 427 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 427 J/m | ASTM D256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1495 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1495 J/m | ASTM D4812 |
Zugfestigkeit | 23.0 °C | 162 MPa Show Supplier Material materials with Zugfestigkeit of 162 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | It is used in automotive fuel pipes, brake brakes, air conditioning pipes, pneumatic equipment hoses, industrial high-pressure hydraulic pipe, pipe fittings, anti-lock solenoid system, precision gear, cam and bearing glide Anti-static capacitor and IC chip guide, cable sheath, transparent pipe, self-adhesive wire paint, VCD-ROM, printer/DVD-ROM silencer gear, sports shoes, cable ties, tennis Clapping and so on many aspects. | |
Fillers | 50% Long Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 243 - 271 °C, Mould temperature 54 - 93 °C, Pre-drying 2 hrs @ 82 °C, Moisture Content 0.2%, Dew Point -29°C |