Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.65 g/cm³ Show Supplier Material materials with Dichte of 1.65 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 313 MPa Show Supplier Material materials with Biegefestigkeit of 313 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 15.41 GPa Show Supplier Material materials with Biegemodul of 15.41 GPa | ASTM D790 |
Dehnung | 23.0 °C | 1 % Show Supplier Material materials with Dehnung of 1 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 20.92 GPa Show Supplier Material materials with Elastizitätsmodul of 20.92 GPa | ASTM D790 |
Impact strength, Izod notched, ASTM | 23.0 °C | 253 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 253 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 229 MPa Show Supplier Material materials with Zugfestigkeit of 229 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 282 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 282 °C | ASTM D648 | |
Entflammbarkeit | HB ASTM D635, for 1.5mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 - 0.3 % Show Supplier Material materials with Schrumpfung of 0.1 - 0.3 % | ASTM D955, (1/8 in (3.2 mm)section) |
Technological properties
Property | ||
---|---|---|
Application areas | Low voltage switches, Circuit breakers, Mechanical parts, Bicycle accessories etc. | |
Color | Natural, and custom colors | |
Fillers | 50% Glass Fiber | |
Processing methods | Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 304 - 329 °C, Mould temperature 135 - 163 °C, Pre-drying 4 hrs @ 121 °C, Moisture Content 0.05%, Dew Point -32°C |