Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.05 g/cm³ Show Supplier Material materials with Dichte of 1.05 g/cm³ | ASTM D297 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dehnung | 23.0 °C | 500 % Show Supplier Material materials with Dehnung of 500 % | ASTM D412 | ||
Härte, Shore A | 23.0 °C | 70 [-] Show Supplier Material materials with Härte, Shore A of 70 [-] | |||
Zugfestigkeit | 23.0 °C | 7 MPa Show Supplier Material materials with Zugfestigkeit of 7 MPa | ASTM D412 | ||
Impact strength, Izod notched, ASTM | No Break | ||||
Impact strength, Izod unnotched, ASTM | No Break |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | HB |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.3 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.3 [-] | ASTM D150 |
Dissipation factor, 1MHz | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 28 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 28 kV/mm | ASTM D149 |
Volume resistivity | 23.0 °C | 1.00E+19 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+19 Ω·cm | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive interior | |
Fillers | 25% Calcium Carbonate | |
Processing methods | Injection Molding, Extrusion |