Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | ASTM D297 |
Mechanisch
Thermisch
Property | Value |
---|---|
Entflammbarkeit | V-0 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 6.3 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 6.3 [-] | ASTM D150 |
Dissipation factor, 1MHz | 23.0 °C | 0.1 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.1 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | ASTM D149 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & Cable applications | |
Processing methods | Injection Molding, Extrusion |