Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.93 g/cm³ Show Supplier Material materials with Dichte of 0.93 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 620 % Show Supplier Material materials with Dehnung of 620 % | ASTM D412 |
Druckverformungsrest | 23.0 °C | 28 [-] Show Supplier Material materials with Druckverformungsrest of 28 [-] | ASTM D395 |
Härte, Shore A | 23.0 °C | 80 [-] Show Supplier Material materials with Härte, Shore A of 80 [-] | ASTM D2240 |
Zugfestigkeit | 23.0 °C | 12 MPa Show Supplier Material materials with Zugfestigkeit of 12 MPa | ASTM D412 |
Thermisch
Property | Value | Comment |
---|---|---|
Brittleness temperature | -60 °C Show Supplier Material materials with Brittleness temperature of -60 °C | D746 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 37 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 37 g/10min | D1238, 190°C/5kg | |
Schrumpfung | 23.0 °C | 1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Processing methods | Extrusion: Hopper Temperature: 150-170°C, Middle Temperature: 160-180°C, Measurment Temperature: 180-200°C, Front Temperature: 190-210°C, Mold Temperature: 180-200°C, Melt Temperature: 170-190°C, Comp. Ratio:3:1, Screen: 20-60 Mesh - Injection: Rear Temperature: 160-180°C, Middle Temperature: 170-190°C, Front Temperature: 190-220°C, Nozzle Temperature: 190-210°C, Melt Temperature:190-200°C, Mold Temperature: 30-80°C, Speed: 100-200rpm, Back Pressure 0.07 - 0.7Mpa |