Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 120 MPa Show Supplier Material materials with Biegefestigkeit of 120 MPa | |
Dehnung | 23.0 °C | 500 % Show Supplier Material materials with Dehnung of 500 % | ASTM D412 |
Härte, Shore D | 23.0 °C | 50 [-] Show Supplier Material materials with Härte, Shore D of 50 [-] | ASTM D2240 |
Reißfestigkeit | 23.0 °C | 128 kN/m Show Supplier Material materials with Reißfestigkeit of 128 kN/m | ASTM D624 |
Zugfestigkeit | 23.0 °C | 20 MPa Show Supplier Material materials with Zugfestigkeit of 20 MPa | ASTM D412 |
Thermisch
Property | Value | Comment |
---|---|---|
Brittleness temperature | -70 °C Show Supplier Material materials with Brittleness temperature of -70 °C | D746 |
Schmelzpunkt | 195 °C Show Supplier Material materials with Schmelzpunkt of 195 °C | |
Vicat-Erweichungstemperatur | 155 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 155 °C |
Technological properties
Property | ||
---|---|---|
Processing methods | Pre-drying: 100°C for 4-8 hr, Injection temperature: 10-20°C higher than melting temperature, Extrusion and blow temperature: higher than melting temperature |