Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 198 MPa Show Supplier Material materials with Biegefestigkeit of 198 MPa | |
Dehnung | 23.0 °C | 450 % Show Supplier Material materials with Dehnung of 450 % | ASTM D412 |
Härte, Shore D | 23.0 °C | 55 [-] Show Supplier Material materials with Härte, Shore D of 55 [-] | ASTM D2240 |
Reißfestigkeit | 23.0 °C | 147 kN/m Show Supplier Material materials with Reißfestigkeit of 147 kN/m | ASTM D624 |
Zugfestigkeit | 23.0 °C | 23 MPa Show Supplier Material materials with Zugfestigkeit of 23 MPa | ASTM D412 |
Thermisch
Property | Value | Comment |
---|---|---|
Brittleness temperature | -70 °C Show Supplier Material materials with Brittleness temperature of -70 °C | D746 |
Schmelzpunkt | 200 °C Show Supplier Material materials with Schmelzpunkt of 200 °C | |
Vicat-Erweichungstemperatur | 170 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 170 °C |
Technological properties
Property | ||
---|---|---|
Processing methods | Pre-drying: 100°C for 4-8 hr, Injection temperature: 10-20°C higher than melting temperature, Extrusion and blow temperature: higher than melting temperature |