Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.06 g/cm³ Show Supplier Material materials with Dichte of 1.06 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 480 % Show Supplier Material materials with Dehnung of 480 % | ASTM D412 |
Härte, Shore A | 23.0 °C | 80 [-] Show Supplier Material materials with Härte, Shore A of 80 [-] | ASTM D2240 |
Zugfestigkeit | 23.0 °C | 8.5 MPa Show Supplier Material materials with Zugfestigkeit of 8.5 MPa | ASTM D412 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL94 V-0 (3mm) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | min., ASTM D149 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | min., ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & Cable applications | |
Processing methods | Hopper Temperature: 150-170°C, Transmission Temperature: 180-200°C, Measurement Temperature: 200-230°C, Die Temperature: 190-220°C |