Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.41 g/cm³ Show Supplier Material materials with Dichte of 8.41 g/cm³ |
Abmessung
Property | Value |
---|---|
Außendurchmesser | 19.1 - 406 mm Show Supplier Material materials with Außendurchmesser of 19.1 - 406 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 3 - 10 % Show Supplier Material materials with Dehnung of 3 - 10 % |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa |
Streckgrenze Rp 0,2 | 23.0 °C | 860 - 1070 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 860 - 1070 MPa |
Zugfestigkeit | 23.0 °C | 1030 - 1310 MPa Show Supplier Material materials with Zugfestigkeit of 1030 - 1310 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Schmelzpunkt | 870 °C Show Supplier Material materials with Schmelzpunkt of 870 °C | |
Wärmeleitfähigkeit | 23.0 °C | 105 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 105 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 25 - 30 % IACS Show Supplier Material materials with Specific Electrical conductivity of 25 - 30 % IACS | |
spezifischer Widerstand | 23.0 °C | 5.8E-6 - 6.9E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.8E-6 - 6.9E-6 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Beryllium | 1.6 - 1.85 % Show Supplier Material materials with Beryllium of 1.6 - 1.85 % | ||
Eisen | 0.6 % Show Supplier Material materials with Eisen of 0.6 % | max., Nickel + Cobalt + Iron | |
Kobalt | 0.2 % Show Supplier Material materials with Kobalt of 0.2 % | min. Nickel + Cobalt | |
Kupfer | Balance | ||
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | min. Nickel + Cobalt |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 165 tube is used in crucial telecommunications applications including undersea instrument housings and repeater housings. |