Streckgrenze Rp 0,2: 860 - 1070 MPa

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Unclassified Low Alloy Steel

ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Chromium Iron Alloy

VDM® Alloy 718

Geliefert von:

VDM Metals

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TB00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TH04

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

ASTM B441 Grade C17500 TH04

Austenitischer rostfreier Stahl

UGI® 209 Solution Annealed

Geliefert von:

Ugitech

Aushärtbarer Stahl

UGI® 4545 AIR H1025

Geliefert von:

Ugitech

Martensitischer Edelstahl

UGI 4418 AIR QT1100

Geliefert von:

Ugitech

Martensitischer Edelstahl

UGI 4418 AIR QT1150

Geliefert von:

Ugitech

Aushärtbarer Stahl

UGI® 4545 AIR H925

Geliefert von:

Ugitech

Aushärtbarer Stahl

UGI® 4545 AIR H1075

Geliefert von:

Ugitech

Martensitischer Edelstahl

UGI 4418 QT900 Drawn Bar

Geliefert von:

Ugitech

Alpha-Beta-Legierung

DIN 17851 Grade 3.7185
Seite 1 von 13