Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dauerfestigkeit | 23.0 °C | 240 MPa Show Supplier Material materials with Dauerfestigkeit of 240 MPa | 10⁷ cycles, R=-1 |
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Supplier Material materials with Elastizitätsmodul of 120 GPa | |
Härte, Rockwell C | 23.0 °C | 30 [-] Show Supplier Material materials with Härte, Rockwell C of 30 [-] | |
Kerbschlagenergie | 23.0 °C | 20 J Show Supplier Material materials with Kerbschlagenergie of 20 J | |
Streckgrenze Rp 0,2 | 23.0 °C | 720 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 720 MPa | |
Zugfestigkeit | 23.0 °C | 790 MPa Show Supplier Material materials with Zugfestigkeit of 790 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.62E-5 1/K |
Schmelzpunkt | 925 °C Show Supplier Material materials with Schmelzpunkt of 925 °C | |
Spezifische Wärmekapazität | 100.0 °C | 390 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 390 J/(kg·K) |
Wärmeleitfähigkeit | 100.0 °C | 70 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 70 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Kupfer | Balance |
Nickel | 8.5 - 9.5 % Show Supplier Material materials with Nickel of 8.5 - 9.5 % |
Zinn | 5.5 - 6.5 % Show Supplier Material materials with Zinn of 5.5 - 6.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | MoldMAX XL Alloy is used as injection mold cores and cavities. |