Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TF00Wrought Copper High Copper Alloy
ASTM B441 Grade C17500 TH04Wrought Copper High Copper Alloy
ASTM B9 Grade C17510 TB00Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 HT, Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 HT, Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B534 Grade C17510 TD04Alpha-Beta-Legierung
DIN 17851 Grade 3.7185Alpha-Beta-Legierung
DIN 17851 Grade 3.7185