Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.83 g/cm³ Show Supplier Material materials with Dichte of 8.83 g/cm³ |
Abmessung
Property | Value |
---|---|
Außendurchmesser | 9.5 - 76 mm Show Supplier Material materials with Außendurchmesser of 9.5 - 76 mm |
Wall thickness | Typically 10 to 20% of OD |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % |
427.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | |
Elastizitätsmodul | 23.0 °C | 138 GPa Show Supplier Material materials with Elastizitätsmodul of 138 GPa |
Härte, Rockwell B | 23.0 °C | 92 [-] Show Supplier Material materials with Härte, Rockwell B of 92 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 585 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 585 MPa |
427.0 °C | 450 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 450 MPa | |
Zugfestigkeit | 20.0 °C | 690 MPa Show Supplier Material materials with Zugfestigkeit of 690 MPa |
427.0 °C | 515 MPa Show Supplier Material materials with Zugfestigkeit of 515 MPa | |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.76E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.76E-5 1/K | |
Schmelzpunkt | 1010 °C Show Supplier Material materials with Schmelzpunkt of 1010 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 414 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 414 J/(kg·K) | at 25°C |
Wärmeleitfähigkeit | 23.0 °C | 225 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 225 W/(m·K) | at 25°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 45 - 55 % IACS Show Supplier Material materials with Specific Electrical conductivity of 45 - 55 % IACS | |
spezifischer Widerstand | 23.0 °C | 2.6E-6 - 3.2E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.6E-6 - 3.2E-6 Ω·m |
Chemical properties
Property | Value |
---|---|
Beryllium | 0.4 - 0.7 % Show Supplier Material materials with Beryllium of 0.4 - 0.7 % |
Kobalt | 2 - 2.7 % Show Supplier Material materials with Kobalt of 2 - 2.7 % |
Kupfer | Balance |
Zirkonium | 0.12 - 0.4 % Show Supplier Material materials with Zirkonium of 0.12 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | High performance powertrain automotive applications such as exhaust valve seats. |