Specific Electrical conductivity: 45 - 55 % IACS

Quick Comparison

Wrought Copper Nickel Grade

UNS C70260 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70250 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18400 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18160 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18150 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Pure / Low Alloyed Copper

UNS C14415 boway

Geliefert von:

Ningbo Boway Alloy Material

3000 Serie

AA Standards Grade 3003 O

Geliefert von:

2 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

UNS C19210 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70318 boway

Geliefert von:

Ningbo Boway Alloy Material

6000 Serie

AA Standards Grade 6063 T1

Geliefert von:

2 Matmatch-Lieferanten

6000 Serie

AA Standards Grade 6063 T5

Geliefert von:

2 Matmatch-Lieferanten

6000 Serie

AA Standards Grade 6063 T6

Geliefert von:

2 Matmatch-Lieferanten

2000 Serie

AA Standards Grade 2011 T8

Geliefert von:

1 Matmatch-Lieferant

6000 Serie

AA Standards Grade 6061 O

Geliefert von:

2 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

5000 Serie

AA Standards Grade 5005 O

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

AA Standards Grade 2024 O

Geliefert von:

1 Matmatch-Lieferant