Titanium

Want to keep this datasheet? Save it now in your required format

Description

Titanium is known for its high strength-to-weight ratio, being stronger than iron and only half as dense. It is one of the best structural materials for the automotive, aerospace and marine industries thanks not only to its strength, but also to its corrosion resistance. It tarnishes at high temperature if exposed to air, but it can be polished to an attractive sheen that will last for years, even in marine and salt-water environments. Apart from these physical and chemical processes, it is also a very biocompatible material that is seldom rejected by body tissues, making it the material of choice for bone implants.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

4.54 g/cm³

Show Material materials with Dichte of 4.54 g/cm³

Mechanisch

PropertyTemperatureValue

Elastizitätsmodul

20.0 °C

116 GPa

Show Material materials with Elastizitätsmodul of 116 GPa

Härte, Brinell

20.0 °C

715 [-]

Show Material materials with Härte, Brinell of 715 [-]

Poissonzahl

20.0 °C

0.32 [-]

Show Material materials with Poissonzahl of 0.32 [-]

Zugfestigkeit

20.0 °C

434 MPa

Show Material materials with Zugfestigkeit of 434 MPa

Thermisch

PropertyTemperatureValue

Schmelzpunkt

1668 °C

Show Material materials with Schmelzpunkt of 1668 °C

Spezifische Wärmekapazität

20.0 °C

520 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 520 J/(kg·K)

Wärmeleitfähigkeit

20.0 °C

22 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 22 W/(m·K)

Elektrisch

PropertyTemperatureValue

spezifischer Widerstand

20.0 °C

4E-9 Ω·m

Show Material materials with spezifischer Widerstand of 4E-9 Ω·m