Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 1.56 g/cm³ Show Material materials with Dichte of 1.56 g/cm³ |
Sauerstoffindex | 20.0 °C | 68 % Show Material materials with Sauerstoffindex of 68 % |
Water content | 20.0 °C | 0.6 % Show Material materials with Water content of 0.6 % |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 2.5 % Show Material materials with Dehnung of 2.5 % |
Druckfestigkeit | 20.0 °C | 561 MPa Show Material materials with Druckfestigkeit of 561 MPa |
Elastizitätsmodul | 20.0 °C | 270 GPa Show Material materials with Elastizitätsmodul of 270 GPa |
Zugfestigkeit | 20.0 °C | 5800 MPa Show Material materials with Zugfestigkeit of 5800 MPa |
Thermisch
Elektrisch
Technological properties
Property | ||
---|---|---|
Application areas | Protective cloth: Firefighter garmants, Safety gloves, Heat resistant garments. Sports: Bicycle Spokes, Bicycle tires, Yacht ropes, Tennis Racket, Badminton racket, Snowboard, Rider suits, Racing Car, Bow Strings. Industrial materials: Heat resistant felt, Cable cover for welding machine, Reinforcement for cements. Other: Speaker cone |