Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 1.44 - 1.45 g/cm³ Show Material materials with Dichte of 1.44 - 1.45 g/cm³ |
Sauerstoffindex | 20.0 °C | 29 - 40 % Show Material materials with Sauerstoffindex of 29 - 40 % |
Water content | 20.0 °C | 2 - 7 % Show Material materials with Water content of 2 - 7 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 2.3 - 4.2 % Show Material materials with Dehnung of 2.3 - 4.2 % | at break |
Elastizitätsmodul | 20.0 °C | 60 - 145 GPa Show Material materials with Elastizitätsmodul of 60 - 145 GPa | |
Tenacity | 1.9 - 2.5 N/tex Show Material materials with Tenacity of 1.9 - 2.5 N/tex | ||
Zugfestigkeit | 20.0 °C | 2700 - 3600 MPa Show Material materials with Zugfestigkeit of 2700 - 3600 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 500 °C Show Material materials with Schmelzpunkt of 500 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Optical fiber,cables, hoses, tires, rubber products, ballistic protection, protective clothing, ropes and cables, composites and belts. |