Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Material materials with Dichte of 1.19 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 93.07 MPa Show Material materials with Biegefestigkeit of 93.07 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.3 GPa Show Material materials with Biegemodul of 2.3 GPa | ASTM D790 |
Dehnung | 23.0 °C | 80 % Show Material materials with Dehnung of 80 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 693 J/m Show Material materials with Impact strength, Izod notched, ASTM of 693 J/m | ASTM D256 |
Streckgrenze | 23.0 °C | 66.18 MPa Show Material materials with Streckgrenze of 66.18 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 124 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ASTM D648, unannealed | |
Entflammbarkeit | V-0 for 1.52 mm and 5VA for 3 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 16 g/10min Show Material materials with Schmelzmassenflussrate of 16 g/10min | 300°C/1.2 Kg | |
Schrumpfung | 23.0 °C | 5E-3 - 7E-3 % Show Material materials with Schrumpfung of 5E-3 - 7E-3 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Lighting applications | |
Color | translucent-opaque | |
Processing methods | Injection Molding, Drying Temperature: 120°C, Drying Time: 3-4 hr, Rear Temperature: 250-265°C, Middle Temperature: 265-276°C, Front Temperature: 265-276°C, Nozzle Temperature: 240-265°C, Mold Temperature: 68-93°C, Back Pressure: 0.34-0.68 MPa, Screw Speed: 40-70 rpm |