Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.16 g/cm³ Show Material materials with Dichte of 2.16 g/cm³ | DIN EN ISO 12086 |
Partikelgröße | 430000 nm Show Material materials with Partikelgröße of 430000 nm | ISO 13320, average value | |
Schüttdichte | 23.0 °C | 0.76 g/cm³ Show Material materials with Schüttdichte of 0.76 g/cm³ | DIN EN ISO 60 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 600 % Show Material materials with Dehnung of 600 % | DIN EN ISO 527-3, 0.2 mm film |
Elastizitätsmodul | 23.0 °C | 0.65 GPa Show Material materials with Elastizitätsmodul of 0.65 GPa | DIN EN ISO 527 |
Härte, Shore D | 23.0 °C | 59 [-] Show Material materials with Härte, Shore D of 59 [-] | DIN EN ISO 868 |
Zugfestigkeit | 23.0 °C | 35 MPa Show Material materials with Zugfestigkeit of 35 MPa | DIN EN ISO 527-3, 0.2 mm film |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.2E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | ||
200.0 °C | 1.4E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
260.0 °C | 1.7E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
Wärmeleitfähigkeit | 23.0 °C | 0.22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.22 W/(m·K) | DIN 52612 | ||
Entflammbarkeit | V-0 UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 82 kV/mm Show Material materials with Durchschlagfestigkeit of 82 kV/mm | DIN EN ISO 12086, 0.2 mm film |
Surface resistivity | 23.0 °C | 1.00E+17 Ω/sq Show Material materials with Surface resistivity of 1.00E+17 Ω/sq | IEC 60093 |
spezifischer Widerstand | 23.0 °C | 1.00E+16 Ω·m Show Material materials with spezifischer Widerstand of 1.00E+16 Ω·m | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 3.5 % Show Material materials with Schrumpfung of 3.5 % | Internal Dyneon method, Cylinder 45 mm diameter |
Technological properties
Property | ||
---|---|---|
Application areas | 3M™ Dyneon™ TFM™ Modified PTFE Granules TFM 1610 is suitable for shaped parts, isostatically moulded pump linings or automatic moulded goods enabling applications like static seals for highly demanding pumps or sealing elements for fittings. Furthermore due to its good elasticity the product enables special processing technologies like deep-drawing orblow-moulding. |