Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.15 g/cm³ Show Material materials with Dichte of 2.15 g/cm³ | DIN EN ISO 12086 |
Partikelgröße | 450000 nm Show Material materials with Partikelgröße of 450000 nm | ISO 13320, average value | |
Schüttdichte | 23.0 °C | 0.84 g/cm³ Show Material materials with Schüttdichte of 0.84 g/cm³ | DIN EN ISO 60 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 430 % Show Material materials with Dehnung of 430 % | DIN EN ISO 527-3, 0.2 mm film |
Elastizitätsmodul | 23.0 °C | 0.6 GPa Show Material materials with Elastizitätsmodul of 0.6 GPa | DIN EN ISO 527 |
Härte, Shore D | 23.0 °C | 56 [-] Show Material materials with Härte, Shore D of 56 [-] | DIN EN ISO 868 |
Zugfestigkeit | 23.0 °C | 36 MPa Show Material materials with Zugfestigkeit of 36 MPa | DIN EN ISO 527-3, 0.2 mm film |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.2E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | ||
200.0 °C | 1.4E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
260.0 °C | 1.7E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
Wärmeleitfähigkeit | 23.0 °C | 0.22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.22 W/(m·K) | DIN 52612 | ||
Entflammbarkeit | V-0 UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 60 kV/mm Show Material materials with Durchschlagfestigkeit of 60 kV/mm | DIN EN ISO 12086, 0.2 mm film |
Surface resistivity | 23.0 °C | 1.00E+17 Ω/sq Show Material materials with Surface resistivity of 1.00E+17 Ω/sq | IEC 60093 |
spezifischer Widerstand | 23.0 °C | 1.00E+16 Ω·m Show Material materials with spezifischer Widerstand of 1.00E+16 Ω·m | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 2.7 % Show Material materials with Schrumpfung of 2.7 % | Internal Dyneon method, Cylinder 45 mm diameter |
Technological properties
Property | ||
---|---|---|
Application areas | 3MTM DyneonTM PTFE Granules TF 1641 is a free-flowing compression moulding powder for applications like sealings, shaped parts, isostatically moulded articles – e.g. lined pipes and valves – or small parts like valve seats. |