Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.06 g/cm³ Show Material materials with Dichte of 2.06 g/cm³ | ASTM D 4745-06 |
Schüttdichte | 23.0 °C | 0.46 g/cm³ Show Material materials with Schüttdichte of 0.46 g/cm³ | ASTM D 4894-07 |
Mechanisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 1.4 % Show Material materials with Schrumpfung of 1.4 % | ASTM D 4894-07 |
Technological properties
Property | ||
---|---|---|
Application areas | 3MTM DyneonTM PTFE Compound TF 7196 can be used in sealing applications in the chemical processing(CPI) and automotive industries. | |
Fillers | 25% Carbon Fiber |