Allgemein
Property | Value | Comment | |
---|---|---|---|
Dichte | 1.76 g/cm³ Show Material materials with Dichte of 1.76 g/cm³ | ISO 1183 | |
Sauerstoffindex | 65 % Show Material materials with Sauerstoffindex of 65 % | ASTM D2863 | |
Wasserabsorption | 0.04 % Show Material materials with Wasserabsorption of 0.04 % | ISO 62 (Method 1, 24hr @ 23°C), maximum | |
Equilibrium | |||
Saturation |
Mechanisch
Thermisch
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 7 [-] Show Material materials with Dielektrizitätskonstante of 7 [-] | ASTM D150, 1 MHz |
Surface resistivity | 1e+14 Ω/sq Show Material materials with Surface resistivity of 1e+14 Ω/sq | DIN 53483, 23 °C, minimum |
spezifischer Widerstand | 1e+12 Ω·m Show Material materials with spezifischer Widerstand of 1e+12 Ω·m | DIN 53483, minimum |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 15.5 g/10min Show Material materials with Schmelzmassenflussrate of 15.5 g/10min | ASTM D1238, 230 °C, 5kg, 2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | PVDF 315080003 is ideal for insulation and buffering materials for wire and cable applications and for tubing. | |
Processing methods | Injection Molding |