Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Schüttdichte | 23.0 °C | 0.6 g/cm³ Show Material materials with Schüttdichte of 0.6 g/cm³ | ASTM D 1895 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 72 MPa Show Material materials with Biegefestigkeit of 72 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.53 GPa Show Material materials with Biegemodul of 3.53 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2 % Show Material materials with Dehnung of 2 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 2.25 GPa Show Material materials with Elastizitätsmodul of 2.25 GPa | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 94 [-] Show Material materials with Hardness, Rockwell L of 94 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 12 J/m Show Material materials with Impact strength, Izod notched, ASTM of 12 J/m | ASTM D256A |
Zugfestigkeit | 23.0 °C | 40 MPa Show Material materials with Zugfestigkeit of 40 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 14 g/10min Show Material materials with Schmelzmassenflussrate of 14 g/10min | ASTM D 1238 | 230°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Multi purpose injection moulding |